10 questions, graded as you go, with the reason for every answer. Start free, no sign-up.
Sample questions
Which material belongs directly behind a segmental retaining wall block as the drainage zone?
The clay excavated from the footing trench
Fine sand mixed with topsoil
Rounded pea gravel mixed with clay fines
Clean, angular crushed stone
Show the answer
D. Clean, angular crushed stone
Clean crushed stone has open voids, so water drains down to the pipe and does not build pressure. Clay and soil holding fines trap water and add load to the wall. Angular stone also interlocks and stays put.
Reference: NCMA Design Manual for Segmental Retaining Walls (drainage)
How should aggregate base be compacted when the finished base will be 8 inches thick?
In thin lifts, compacted each pass
In one 8-inch layer with a single pass
Left loose so it can drain better
Soaked until it pools, then raked flat
Show the answer
A. In thin lifts, compacted each pass
A plate compactor only reaches so deep, so thick layers stay loose underneath and settle later. Thin lifts compacted one at a time give a dense, even base. Loose or flooded stone will not carry load.
Reference: ICPI Tech Spec 2, Construction of Interlocking Concrete Pavements
A finisher wants to add water to a stiff load of concrete to make it easier to float. What is the problem with doing that?
It makes the concrete set before it can be finished
It makes the slab too hard to cure
It weakens concrete and increases cracking
It changes the color but not the strength
Show the answer
C. It weakens concrete and increases cracking
Extra water beyond the design raises the water-cement ratio, which weakens the hardened concrete, increases shrinkage and reduces durability. The better fix is a workability-improving admixture ordered from the plant.
Reference: ACI 302.1R, guide to concrete floor and slab construction (water-cement ratio, finishing)